Main reason:
1.The substrate has oil, water, dust and stains.
2.The base metal surface is too smooth or without polished.
3.The underly paint has been aging, chalking and brittle rupture.
Precaution:
1.Ensure the surface is completely clean.
2.After spraying, use the sandpaper to polish the metal surface and spray antirust primer.
3.Remove the old paint and then paint.
Correction method:
Remove the peeling part and the surrounding weak attachment part and then use the P800 sandpaper to polish and spray again.